Abu biyu, tetra fluorocarbon resin, aliphatic isocyanate warkewa topcoat, yanayi mai kyau, riƙe launi da juriya na sinadarai, aikin tsabtace kai.
Siffofin
1.Highly ado, super anti-ultraviolet yi, m yanayin juriya;
2. Fim ɗin fenti yana da haske da tsabta, ba sauƙin da za a lalata shi da datti, kuma yana da kyakkyawan aikin tsaftacewa.
3.High daskararru da low VOC, babu chlorine, fluorine abun ciki na ƙarfi mai narkewa al'amari ne ba kasa da 24%.
4.Excellent sunadarai juriya, mai kyau permeability juriya, fice lalata juriya.
An shawarar amfani
Kyakkyawan kariyar masana'antu da ƙayyadaddun kayan ado, dacewa da sifofin ƙarfe ko saman kankare a cikin yanayin yanayi daban-daban, kamar manyan sifofin ƙarfe, gadoji, dandamali na teku, bangon waje na tankunan ajiya, manyan kayan jirgi, kayan aikin petrochemical, da kayan aikin injiniya, da sauransu. Ya dace musamman don filaye tare da manyan buƙatu don mai sheki da riƙe launi.
Umarnin aikace-aikace
Abubuwan da ake amfani da su na Jiyya na Substrate da Surface:
Yi amfani da ma'aunin tsaftacewa mai dacewa don cire duk maiko da datti a saman ƙasa, da kiyaye farfajiyar tsabta, bushe da rashin ƙazanta.
Dole ne a yi amfani da wannan samfurin akan abin da aka ba da shawarar maganin tsatsa a cikin ƙayyadadden tazarar dawowa.
ɓangarorin da suka lalace na firam ɗin dole ne a busa su zuwa Sa.2.5 (ISO8501-1) ko kuma a bi da su zuwa ma'aunin St3, kuma ya kamata a yi amfani da fenti na farko zuwa waɗannan sassan.
Aiwatar da Magani
1.Substrate surface dole ne a kiyaye tsabta da bushe, da kuma zafin jiki na substrate dole ne 3 ° C sama da raɓa batu don kauce wa condensation.
2.Wannan samfurin kuma za'a iya amsawa kuma a warke shi a yanayin zafi kamar -10 ° C, idan dai babu sanyi a saman.
An haramta aikace-aikacen waje a cikin yanayi mai tsanani kamar ruwan sama, hazo, dusar ƙanƙara, iska mai ƙarfi da ƙura mai nauyi.
4.The zafin jiki ne high a lokacin rani, yi hankali da bushe spraying, da kuma ci gaba da samun iska
5.lokacin aikace-aikace da lokacin bushewa a cikin kunkuntar wurare.
Rayuwar tukunya
5 ℃ | 15 ℃ | 25 ℃ | 35 ℃ |
6h ku. | 5 h. | 4 h. | 2.5h. |
Aikace-aikace
Ya dace da overcoating a baya coatings kamar epoxy ko polyurethane, da kuma amfani da matsayin m high-ado weather-resistant topcoat ga karfe Tsarin ko kankare saman a daban-daban yanayi yanayi.
Rayuwar tukunya
Hanyar aikace-aikace | Naúrar | Fesa mara iska | Fesa iska | Brush/Roller |
Nozzle Orifice | mm | 0.35 zuwa 0.53 | 1.5 zuwa 2.5 | -- |
Matsin bututun ƙarfe | kg/cm2 | 150 ~ 200 | 3 zuwa 4 | -- |
Siriri | % | 0 ~ 10 | 10 zuwa 25 | 5 zuwa 10 |
Bushewa & Magance
Substrate zafin jiki | -5 ℃ | 5 ℃ | 15 ℃ | 25 ℃ | 35 ℃ |
Surface-bushe | 2hrs. | 1 hr | 45 min | 30 min | 20 min |
Ta-bushe | 48h ku. | 24 h. | 12h. | 8h ku. | 4h |
Min.Lokacin sake dawowa | 36 h. | 24 h. | 12h. | 8h ku. | 4h |
Max.Lokacin sake dawowa | Kwanaki 30 |
Gabatarwa & Sakamakon shafa
Fenti na gaba:kowane irin epoxy, polyurethane tsaka-tsakin fenti ko rigar tsatsa, da fatan za a tuntuɓi Zindn
Shiryawa & Ajiya
shiryawa:tushe 25kg, curing wakili 2.5kg
Wurin walƙiya:> 25 ℃
Ajiya:Dole ne a adana shi daidai da dokokin ƙananan hukumomi.Ajiya
muhalli ya zama bushe, sanyi, samun iska mai kyau kuma nesa da zafi da tushen wuta.The
Dole ne a kiyaye ganuwar marufi sosai a rufe.
Rayuwar rayuwa:Shekara 1 a ƙarƙashin kyakkyawan yanayin ajiya daga lokacin samarwa.